Standards
TS EN ISO 24373
|
S Cu 7061(CuNi1O) |
EN ISO 24373
|
S Cu 7061(CuNi1O) |
DIN 1733
|
SG-CuNi10 Fe |
Chemical Composition of Welding Wire% (Typical)
Cu
|
Rest |
Mn
|
1.00 |
Ni
|
10.00 |
Ti
|
0.17 |
Fe
|
1.80 |
Typical Base Material Grades
- CUNIFER 30, CUNIFER 40, Cu90-Ni10 and lo w Ni Alloys Cu-Ni alloys
- (2.0862) CuNi5Fe, (2.0872) CuNi10Fe
Mechanical Properties
Yield Strength (N/mm²) |
Tensile Strength (N/mm²) |
Elongation ((Lo=5do) (%)) |
Hardness (as welded) (HB) |
150 |
350 |
30 |
200 |
Features and Applications
- It is used for copper nickel alloys with 10% nickel such as CuNi5Fe, CuNi10Fe.
- Weld deposit is highly corrosion resistant
- It is used for joining and surfacing copper-nickel alloys and CuNiFe pipes which pertorm in corrosive areas such as seawater
- Shielding Gas: Ar
Welding Positions
Welding Method
Operating Data
Product Code |
Diametré x Length (mm) |
Diameter x Length (inch) |
Package Weight (Kg) |
6031100258 |
Ø1.60 x 1000 |
Ø1/16 x 39 |
5 |
6031100259 |
Ø2.00 x 1000 |
Ø5 /64 x 39 |
5 |
6031100385 |
Ø2.40 x 1000 |
Ø3/32 x 39 |
5 |
6031100260 |
Ø3.20 x 1000 |
Ø1/8 x 39 |
5 |
Approvals