Standards
TS EN ISO 14343-A
|
G 23 12 L Si |
EN ISO 14343-A
|
G 23 12 L Si |
AWS A5.9
|
ER 309 L Si |
Chemical Composition of Welding Wire% (Typical)
C
|
0.03 |
Si
|
0.80 |
Mn
|
1.80 |
Cr
|
23.50 |
Ni
|
13.00 |
Typical Base Material Grades
- Ferritic Cr and austenitic CrNi steels, austenitic manganese steels, unalloyed high strength steels, high temperature steels
Mechanical Properties
Yield Strength (N/mm²) |
Tensile Strength (N/mm²) |
Impact Strength (ISO-V/+20°C) |
Elongation ((Lo=5do) (%)) |
min. 320 |
min. 520 |
min. 47 J |
min. 30 |
Features and Applications
- Applicability on ferritic Cr or austenitic CrNi steels, austenitic manganese steels, unalloyed high-strength steels, heat-treated steels
- Usability in welding austenitic stainless steels, in joint- welding of different kinds of metals, in buffer layers, in joint-welding of corrosion-resistant stainless steels to each other or to low-alloyed steels, and in welding coated steels
- Ar+ %2.5 O2 or (Ar+%2.5 CO2) gas is used as shielding gas
Welding Positions
Welding Method
Operating Data
Product Code |
Package Type |
Weight (Kg) |
Diameter (mm) |
Diameter (inch) |
6011100383 |
BS 300 Spool |
12.5 |
Ø0.80 |
Ø0.030 |
6011100331 |
BS 300 Spool |
15 |
Ø1.00 |
Ø0.040 |
6011100332 |
BS 300 Spool |
15 |
Ø1.20 |
Ø0.047 |
Approvals