Stainless Steel Electrode - ELOX RS 307
Standards
EN ISO 3581-A
|
E Z 18 9 MnMo R 5 3 |
TS EN ISO 3581-A
|
E Z 18 9 MnMo R 5 3 |
AWS A5.4
|
~E307-26 |
Chemical Composition of Weld Metal % (Typical)
C |
Si |
Mn |
Cr |
Ni |
Mo |
0,07 |
0,9 |
5,6 |
19,0 |
8,5 |
0,75 |
Typical Base Material Grades
- Dissimilar joints, tough buffer and intermediate layers prior to hardfacing, 14Mn-steels, 13 – 17% Cr and heat resistant Cr and austenitic steels up to 850ºC, armor plates, high carbon and quenched and tempered steels, surfacing of gears, valves, turbine blades, etc. For joint welding of unalloyed / low-alloyed or Cr steels with high-alloyed Cr and CrNi-steels. Welding of austenitic high manganese steels and with other steels.
Mechanical Properties
Yield Strength (N/mm²) |
Tensile Strength (N/mm²) |
Impact Strength (ISO-V/+20°C) |
Elongation ((Lo=5do) (%)) |
min.400 |
590 - 700 |
min.47J |
min.35 |
Features and Applications
- Welding of high resistant alloyed / unalloyed steels, heat resistant steels / stainless steels, steels wit 14%Mn, for problematic steels.
- Joint and filler welding of different metals.
- Rutile coated electrode, weld metal is austenitic, resistant to thermal shocks, keeps its thoughness down to -100 ºC.
- Re-drying: 120-200ºC / 2 h.
Current Type
Welding Positions
Operating Data
Product Code |
Diametré x Length (mm) |
Diameter x Length (inch) |
Welding Current (A) |
Weight g / 100 pcs |
3010100943 |
ø3,2 x 350 |
ø1/8 x 14 |
110 - 150 |
4900 |
3010100948 |
ø4,0 x 350 |
ø5/32 x 14 |
140 - 180 |
7830 |
3010100953 |
ø5,0 x 350 |
ø3/16 x 14 |
180 - 220 |
11700 |
Approvals